Acta Metallurgica Sinica (English Letters) ›› 2019, Vol. 32 ›› Issue (9): 1075-1088.DOI: 10.1007/s40195-019-00920-4
• Orginal Article • Previous Articles Next Articles
Li Jun-Lei1, Wang Shuai1, Cao Fang1, Lin Xiao2, Wei Xiao-Wei1, Zhao Zhen-Hua1, Dou Xiao-Jie1, Yu Wei-Ting1, Yang Ke3(), Zhao De-Wei1(
)
Received:
2019-03-15
Revised:
2019-04-03
Online:
2019-09-10
Published:
2019-08-06
Li Jun-Lei, Wang Shuai, Cao Fang, Lin Xiao, Wei Xiao-Wei, Zhao Zhen-Hua, Dou Xiao-Jie, Yu Wei-Ting, Yang Ke, Zhao De-Wei. Fabrication and Characterization of Nanopillar-Like HA Coating on Porous Ti6Al4V Scaffold by a Combination of Alkali-Acid-Heat and Hydrothermal Treatments[J]. Acta Metallurgica Sinica (English Letters), 2019, 32(9): 1075-1088.
Add to citation manager EndNote|Ris|BibTeX
Fig. 1 a 3D digital model of the diamond unit cell, b 3D digital model of the cylindrical porous Ti6Al4V, c macrophotograph of the cylindrical porous Ti6Al4V fabricated by AM, dSEM image of the porous Ti6Al4V fabricated by AM
Properties | Values |
---|---|
Strut diameter (μm) | 408.3?±?8.8 |
Porosity (%) | 67.9?±?1.1 |
Max pore size (μm) | 691?±?11.2 |
Compressive strength (MPa) | 82.1?±?3.7 |
Elastic modulus (GPa) | 4.2?±?0.1 |
Table 1 Structural and mechanical properties of the porous Ti6Al4V
Properties | Values |
---|---|
Strut diameter (μm) | 408.3?±?8.8 |
Porosity (%) | 67.9?±?1.1 |
Max pore size (μm) | 691?±?11.2 |
Compressive strength (MPa) | 82.1?±?3.7 |
Elastic modulus (GPa) | 4.2?±?0.1 |
Fig. 2 a Pictures of the porous Ti6Al4V, AH-porous Ti6Al4V and HT/AH-porous Ti6Al4V; b surface morphology of HT/AH-porous Ti6Al4V; c cross section of coating on HT/AH-porous Ti6Al4V; d EDS analysis of the elements found on the surface of HT/AH-porous Ti6Al4V
Fig. 4 Ultrapure water and glycerol contact angle measurement on the porous Ti6Al4V substrate (a, d), AH-porous Ti6Al4V coating (b, e), HT/AH-porous Ti6Al4V coating (c, f)
Samples | Mean CA (°) | Mean SFE (mJ/m2) | |
---|---|---|---|
Ultrapure water | Glycerol | ||
Porous Ti6Al4V | 91.7?±?1.7 | 72.6?±?0.5 | 52.2?±?3.1 |
AH-porous Ti6Al4V | 48.6?±?0.6 | 36.2?±?1.1 | 61.7?±?2.3 |
HT/AH-porous Ti6Al4V | 22.1?±?1.2 | 2.5?±?0.2 | 65.3?±?1.5 |
Table 2 Mean contact angle (CA) values (±?standard deviation) and mean values (±?standard deviation) of the total surface-free energy (SFE) of the porous Ti6Al4V, AH-porous Ti6Al4V and HT/AH-porous Ti6Al4V
Samples | Mean CA (°) | Mean SFE (mJ/m2) | |
---|---|---|---|
Ultrapure water | Glycerol | ||
Porous Ti6Al4V | 91.7?±?1.7 | 72.6?±?0.5 | 52.2?±?3.1 |
AH-porous Ti6Al4V | 48.6?±?0.6 | 36.2?±?1.1 | 61.7?±?2.3 |
HT/AH-porous Ti6Al4V | 22.1?±?1.2 | 2.5?±?0.2 | 65.3?±?1.5 |
Fig. 6 SEM photographs and EDS analysis of surfaces of porous Ti6Al4V (a-c), AH-porous Ti6Al4V (d-f), HT/AH-porous Ti6Al4V (g-i) immersed in SBF for 7 days
Fig. 7 A Concentrations of Ca2+ (a) phosphate (b) ions measured by ICP, which were released from porous Ti6Al4V, AH-porous Ti6Al4V and HT/AH-porous Ti6Al4V as a function of soaking time in deionized water; B influence of surface treatment on fibronectin (a) vitronectin (b) adsorption, n?=?3, asterisks (*) indicate statistical significance, p?<?0.05
Fig. 8 a Measurement of MSCs proliferation by CCK-8 assay after 1, 4 and 7 days incubation. For each group, n?=?3; asterisks (*) indicate statistical significance, p?<?0.05; bmorphology of MSCs adhesions on porous Ti6Al4V, AH-porous Ti6Al4V and HT/AH-porous Ti6Al4V surfaces after 24 h of cell culture; c live/dead staining of MSCs on surfaces of porous Ti6Al4V, AH-porous Ti6Al4V and HT/AH-porous Ti6Al4V after 7 and 14 days of cell cultures
Fig. 9 a ALP activities of MSCs incubated for 7, 14 and 21 days on surfaces of porous Ti6Al4V, AH-porous Ti6Al4V and HT/AH-porous Ti6Al4V; b relative mRNA expressions of ALP, Col-1, OCN, Runx2 and OPN after 7, 14 and 21 days of cell cultures, n?=?3, asterisks (*) indicate statistical significance, p?<?0.05
The ratio of OD value | porous Ti6Al4V | AH-porous Ti6Al4V | HT/AH-porous Ti6Al4V |
---|---|---|---|
Day 4/Day 1 | 2.214 | 1.854 | 1.909 |
Day 7/Day 4 | 1.309 | 1.308 | 1.472 |
Table 3 Ratio of OD values between different groups after cultures for 1, 4 and 7 days
The ratio of OD value | porous Ti6Al4V | AH-porous Ti6Al4V | HT/AH-porous Ti6Al4V |
---|---|---|---|
Day 4/Day 1 | 2.214 | 1.854 | 1.909 |
Day 7/Day 4 | 1.309 | 1.308 | 1.472 |
|
[1] | Li-Sha Wang, Jing-Hua Jiang, Bassiouny Saleh, Qiu-Yuan Xie, Qiong Xu, Huan Liu, Ai-Bin Ma. Controlling Corrosion Resistance of a Biodegradable Mg-Y-Zn Alloy with LPSO Phases via Multi-pass ECAP Process [J]. Acta Metallurgica Sinica (English Letters), 2020, 33(9): 1180-1190. |
[2] | Guercio Giuseppe Del, Manuela Galati, Abdollah Saboori, Paolo Fino, Luca Iuliano. Microstructure and Mechanical Performance of Ti-6Al-4V Lattice Structures Manufactured via Electron Beam Melting (EBM): A Review [J]. Acta Metallurgica Sinica (English Letters), 2020, 33(2): 183-203. |
[3] | Jiahua Zhang, Yi Yang, Sheng Cao, Zhiqiang Cao, Dmytro Kovalchuk, Songquan Wu, Enquan Liang, Xi Zhang, Wei Chen, Fan Wu, Aijun Huang. Fine equiaxed β grains and superior tensile property in Ti-6Al-4V alloy deposited by coaxial electron beam wire feeding additive manufacturing [J]. Acta Metallurgica Sinica (English Letters), 2020, 33(10): 1311-1320. |
[4] | Wen Wang, Peng Han, Pai Peng, Ting Zhang, Qiang Liu, Sheng-Nan Yuan, Li-Ying Huang, Hai-Liang Yu, Ke Qiao, Kuai-She Wang. Friction Stir Processing of Magnesium Alloys: A Review [J]. Acta Metallurgica Sinica (English Letters), 2020, 33(1): 43-57. |
[5] | Zhao Zhang, Zhi-Jun Tan, Jian-Yu Li, Yu-Fei Zu, Jian-Jun Sha. Integrated Modeling of Process-Microstructure-Property Relations in Friction Stir Additive Manufacturing [J]. Acta Metallurgica Sinica (English Letters), 2020, 33(1): 75-87. |
[6] | Xiao Lin, Adrian Chan, Xiao-Xiao Tan, Hui-Lin Yang, Lei Yang. Fabrication and Characterizations of Metallic Mg Containing PMMA-Based Partially Degradable Composite Bone Cements [J]. Acta Metallurgica Sinica (English Letters), 2019, 32(7): 808-816. |
[7] | K. Jurczyk, A. Miklaszewski, K. Niespodziana, M. Kubicka, M. U. Jurczyk, M. Jurczyk. Synthesis and Properties of Ag-doped Titanium-10 wt% 45S5 Bioglass Nanostructured Scaffolds [J]. Acta Metallurgica Sinica (English Letters), 2015, 28(4): 467-476. |
[8] | Thiagarajan Hemalatha, Gunasekaran Krithiga, Baskar Santhosh Kumar, Thotapalli P. Sastry. Preparation and Characterization of Hydroxyapatite-Coated Selenium Nanoparticles and their Interaction with Osteosarcoma (SaOS-2) Cells [J]. Acta Metallurgica Sinica (English Letters), 2014, 27(6): 1152-1158. |
Viewed | ||||||
Full text |
|
|||||
Abstract |
|
|||||