Acta Metallurgica Sinica (English Letters) ›› 2010, Vol. 23 ›› Issue (1): 50-56.DOI: 10.11890/1006-7191-101-50

• Research paper • Previous Articles     Next Articles

Preparation of an ultrafine-grained Fe-40Al intermetallic compound

Jiqiang MA1,2, Jun YANG1, Qinling BI1,Weimin LIU1   

  1. 1. State Key Laboratory of Solid Lubrication, Lanzhou Institute of Chemical Physics, Chinese Academy of Sciences, Lanzhou 730000, China
    2. Graduate University of Chinese Academy of Sciences, Beijing 100039,China
  • Received:2009-05-22 Revised:2009-07-10 Online:2010-02-25 Published:2010-02-09
  • Contact: Jun YANG

Abstract:

An ultrafine grained Fe-40Al intermetallic compound is fabricated by a self-propagating high temperature synthesis (SHS) casting. The XRD result shows that the Fe-40Al intermetallic compound consists of the B2 FeAl phase. The Fe-40Al intermetallic compound presents ultrafine grain size in the range of 100--600~nm, leading from the high nucleation rate and the low growth rate. The Fe-40Al intermetallic compound exhibits high hardness (3.4 GPa) and high bending strength (830 MPa) and high compressive strength (2700 MPa), which originate from the ultrafine-structure in the material. The effect of the load on dry-sliding wear rate of the material against AISI52100 steel was investigated. The wear rate increases with the increase of normal load. The dominated wear mechanism is microfracture.

Key words: Iron aluminides, Self-propagating high temperature, synthesis (SHS) casting, Ultrafine grain, Preparation, Wear