Acta Metallurgica Sinica (English Letters) ›› 1992, Vol. 5 ›› Issue (9): 201-205.

• Research paper • Previous Articles     Next Articles

BEHAVIOUR OF BUFFER LAYER IN JOINING OF SIALON CERAMICS TO STEEL 40Cr

XIAN Aiping SI Zhongyao Institute of Metal Research,Academia Sinica,Shenyang,China Doctoral Candidate,Laboratory of Welding and Joining,Institute of Metal Research,Academia Sinica,Shenyang 110015,China   

  • Received:1992-09-11 Revised:1992-09-11 Online:1992-09-11 Published:2009-10-10

Abstract: The buffer layer material itself may be influential to the bond strength between active brazing filler and ceramics.For Ag_(57)Cu_(38)Ti_5 filler metal,Cu or Ta is excellent buffer layer material, but Kovar or Ni-15Cr-15Co is worse.It was important to design a layer of soft buffer,such as Cu,to relax interfacial stress rather than hard buffer layer,such as Mo,to avoid stress. There is an optimum thickness range of soft buffer layer,saying h/L=0.02—0.1. It was a good solution to the interfacial stress problem to use soft/hard buffer layer to increase metal/ceramics joint strength.Finally,an idea of designing gradual materials as buffer layer between metal and ceramics was suggested.

Key words: ceramic/metaljointing, Sialon, steel 40Cr, active brazing, interlayer