Preternatural Hexagonal High-Entropy Alloys: A Review
Rui-Xuan Li, Jun-Wei Qiao, Peter K. Liaw, Yong Zhang
Table 4 Currently developed single-phase HCP alloys and alloys with HCP structure as the main phase
Published year Composition Structure c/a References
2013 Co25Os25Re25Ru25 HCP (predicted) None [16]
2014 Y20Gd20Tb20Dy20Lu20 HCP + OMP 1.574 [17]
2014 Gd20Tb20Dy20Tm20Lu20 HCP + OMP 1.574 [17]
2014 Ho20Dy20Y20Gd20Tb20 HCP 1.579 [18, 30]
2014 Al20Li20Mg20Sc20Ti20 HCP (annealing) 1.588 [37]
2015 Co25Fe25Re25Ru25 HCP 1.581 [29]
2015 Co25Re25Ru25V25 HCP + OMP 1.606 [29]
2016 Sc16.67Y16.67La16.67Ti16.67Zr16.67Hf16.67 Dual HCP 1.583/1.575 [33]
2016 Gd20Ho20La20Tb20Y20 HCP 1.589 [31]
2017 Al15Hf25Sc10Ti25Zr25 HCP + OMP 1.585 [67]
2017 Ir19Os22Re21Rh20Ru19 HCP 1.590 [32]
2017 Gd20Dy20Er20Ho20Tb20 HCP 1.578 [49]
2017 Co20Cr20Fe20Mn20Ni20 HCP (high pressure) 1.620 [34, 35]
2017 Co20Cr26Fe20Mn20Ni14 HCP (high pressure torsion) 1.620 [36]
2017 Fe50Mn30Co10Cr10 HCP + FCC 1.616 [38]
2018 Ce20Gd20Tb20Dy20Ho20 HCP + OMP 1.588 [68]
2018 Er16.67Gd16.67Ho16.67La16.67Tb16.67Y16.67 HCP 1.578 [43]
2019 Ir26Mo20Rh22.5Ru20W11.5 HCP 1.601 [56]
2019 Ir25.5Mo20Rh20Ru25W9.5 HCP 1.598 [56]