A Comparison Study of Wear and Fretting Fatigue Behavior Between Cr-alloyed Layer and Cr-Ti Solid-solution Layer
Shou-Ming Yu(),Dao-Xin Liu(),Xiao-Hua Zhang,Cheng-Song Liu

.

Fig. 12. Morphologies of the fretting contact zones a, c, e and the fretting fatigue fracture surfaces b, d, f of the shot peened samples: a, b BM + SP sample; c, d BM + Cr + SP sample; e, f Cr-Ti + SP sample