Dynamic Recrystallization Behavior of Bimodal Size SiCp-Reinforced Mg Matrix Composite during Hot Deformation |
Cui-Ju Wang, Kun-Kun Deng, Shan-Shan Zhou, Wei Liang |
Fig. 5 The σc and εc of AZ91 alloy and S-1.5 + 10-8.5 composite compressed at 270-370 °C and 0.01 s-1: a critical stress σc, b critical strain εc |
![]() |