Dynamic Recrystallization Behavior of Bimodal Size SiCp-Reinforced Mg Matrix Composite during Hot Deformation
Cui-Ju Wang, Kun-Kun Deng, Shan-Shan Zhou, Wei Liang
Fig. 8 Optical microstructures of AZ91 alloy and S-1.5 + 10-8.5 composite compressed at 320 °C and 0.01 s-1 with different strains (0.1, 0.2, 0.3 and 0.5)