Secondary Recrystallization Behaviors of Grain-Oriented 6.5 wt% Silicon Steel Sheets Produced by Rolling and Nitriding Processes
Jing Qin, Ping Yang, Wei-Min Mao, Feng Ye, Li Liu
Fig. 6 Distribution of the precipitates at 875 °C a, 900 °C b, and 925 °C c in the surface and the central layer of samples nitrided 60 s and EDS analysis of the precipitates d