Secondary Recrystallization Behaviors of Grain-Oriented 6.5 wt% Silicon Steel Sheets Produced by Rolling and Nitriding Processes |
Jing Qin, Ping Yang, Wei-Min Mao, Feng Ye, Li Liu |
Fig. 4 Local orientation images, {200} pole figures, and ODFs (levels: 1, 2, 4, 8, 10, 20, 40, 80) of the samples, which are nitrided for 60 s and extracted at 850 °C a, 875 °C b, 900 °C c, 925 °C d, 950 °C e, 975 °C f, 1000 °C, g 1050 °C h, and 1075 °C i during the secondary recrystallization annealing |
![]() |