Induced Plasticity of a Brittle (La, Ce)-Based Bulk Metallic Glass by Surface Corrosion
Ji-Juan Liu, Ran Li, Lian-Xiang Fang, Ju Wang, Tao Zhang
Fig. 4 SEM images of the failed (La0.5Ce0.5)65Al10Cu25 glassy rods after compressive fracture for the different immersing time: a, e untreated; b, f 5 min; c, g 20 min; d, h 30 min. The position of the typical selected surface morphologies for each sample, as shown in e-h, is highlighted by rectangle in a-d, respectively