Microstructure Evolution and Residual Stress Redistribution in Selective Laser Melted TA15 Titanium Alloy Under Severe Shot Peening Treatment

Ang Yin1, Wenbo Li1, Chengxi Wang2, Vincent Ji3, Chuanhai Jiang1()   

  1. 1School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 201109, China
    2Faculty of Transportation Engineering, Kunming University of Science and Technology, Kunming 650500, China
    3ICMMO/LEMHE, UMR 8182, Université Paris-Saclay, Bat 410, 91400 Orsay, France
  • Received:2025-03-29 Revised:2025-04-24 Accepted:2025-05-04 Online:2025-11-10 Published:2025-07-29
  • Contact: Chuanhai Jiang, jch2111962@163.com

Abstract:

A gradient nanostructured layer was fabricated on the surface of TA15 (Ti-6Al-2Zr-1Mo-1V) alloy (produced by selective laser melting) using severe shot peening (SSP). This study focuses on the evolution of the microstructure and the mechanism of grain refinement in TA15 titanium alloy during SSP treatment. Transmission electron microscopyand Rietveld refinement methods were employed. The residual stress and microhardness variations with depth were also characterized. The results show: (1) At the initial stage of deformation, plastic deformation is primarily accommodated through twinning and dislocation slip. (2) As the strain increases, twinning disappears, and dislocations interact to form tangles. Some dislocations annihilate and rearrange into subgrain boundaries, subdividing the original grains into subgrains. (3) With continued dislocation activity, the subgrain size decreases until nanocrystals are formed through the dynamic rotational recrystallization. SSP introduced compressive residual stress (CRS) in the near-surface layer of the material, with the maximum CRS of approximately −1141 MPa observed in the subsurface layer. It also induced work hardening, increasing the surface hardness to approximately 479 HV. However, the surface roughness increases, leading to a slight deterioration in surface quality.

Key words: Severe shot peening, Selective laser melting, TA15, Residual stress, Gradient nanostructured layer, Microstructure